Effect Of Curing Methods And Scrap Tyre Addition On Properties Of Mortars
dc.authorid | 187924 | en_US |
dc.authorid | 182054 | en_US |
dc.authorid | 46664 | en_US |
dc.contributor.author | Bostancı, Levent | |
dc.contributor.author | Üstündağ, Özlem | |
dc.contributor.author | Sola, Özlem Çelik | |
dc.contributor.author | Uysal, Mücteba | |
dc.date.accessioned | 2020-10-16T11:10:26Z | |
dc.date.available | 2020-10-16T11:10:26Z | |
dc.date.issued | 2020 | |
dc.department | İstanbul Beykent Üniversitesi | en_US |
dc.description.abstract | Mechanical, thermal conductivity, and porosity properties of scrap tyre incorporated mortars are examined experimentally in this study for various curing conditions. Cement mortars were prepared by adding 0%, 1%, 5%, 10% and 18% of scrap tyre by cement weight, and the mortars were subjected to three curing procedures for 14 weeks. The lowest thermal conductivity values were obtained on samples containing 18% of scrap tyre by water curing and wetting-drying curing as 1.09 and 1.14 W/mK, respectively. The maximum compressive strength of 61.5 MPa was obtained on a pure sample cured by wetting and drying, while the flexural strength of pure and a 1%additive incorporated samples, which were also cured by wetting-drying, amounted to 9.1 and 8.2 MPa, respectively. | en_US |
dc.identifier.citation | GRAĐEVINAR 72 (2020) 4, 311-322 | en_US |
dc.identifier.doi | 10.14256/JCE.2575.2018 | |
dc.identifier.issn | 1748-0221 | |
dc.identifier.scopus | 2-s2.0-85092046023 | en_US |
dc.identifier.scopusquality | Q2 | en_US |
dc.identifier.uri | https://doi.org/10.14256/JCE.2575.2018 | |
dc.identifier.wos | WOS:000534612700002 | en_US |
dc.identifier.wosquality | Q3 | en_US |
dc.indekslendigikaynak | Web of Science | en_US |
dc.indekslendigikaynak | Scopus | en_US |
dc.language.iso | en | en_US |
dc.publisher | Croatian Association of Civil Engineers | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.subject | Mortar | en_US |
dc.subject | Scrap tyre | en_US |
dc.subject | Curing procedure | en_US |
dc.subject | Thermal conductivity | en_US |
dc.subject | Compressive strength | en_US |
dc.title | Effect Of Curing Methods And Scrap Tyre Addition On Properties Of Mortars | en_US |
dc.type | Article | en_US |
Dosyalar
Orijinal paket
1 - 1 / 1
Yükleniyor...
- İsim:
- 91 Effect Of Curing Methods And Scrap Tyre Addition On Properties Of Mortars.pdf
- Boyut:
- 297.14 KB
- Biçim:
- Adobe Portable Document Format
- Açıklama:
Lisans paketi
1 - 1 / 1
Küçük Resim Yok
- İsim:
- license.txt
- Boyut:
- 1.44 KB
- Biçim:
- Item-specific license agreed upon to submission
- Açıklama: